MT-967 Green Electroless Nickel Plating Agent (Low P)
1. Suitable for electroless plating with eco-agent of low phosphorus(6-8%)
2. Highly tarnish resistance with MT-967D addition for brighter effect
3. Quick precipitation speed at 18-23μm/h
4. Stable solution for recycling (10-12 cycles)
Specifications
NiSO4 29g/L
NaH2PO2 18g/L
MT-967A 60mL/L
MT-967B 150mL/L
pH 4.2-4.8
Temperature 85-90℃
Dosage 0.5-2dm2. L(Best at 1.0dm2. L)
Agitation Filtrating Air Agitation
Precipitation Speed 15-20 μm/dm2. h
Surface Area 45-50 μm/dm2. h
Life Span 10-12 Cycles
Click here to download detailed Introduction in PDF